Static and dynamic failure load of fiber-reinforced composite and particulate filler composite cantilever resin-bonded fixed dental prostheses

J Adhes Dent. 2010 Jun;12(3):207-14. doi: 10.3290/j.jad.a17653. ABSTRACT PURPOSE: The aim of this study was to evaluate in vitro the influence of fiber reinforcement and luting cement on the static failure load (SFL) and dynamic failure load (DFL) of simulated two-unit cantilever resin-bonded fixed dental prostheses (RBFDPs). MATERIALS AND METHODS: […]

Post-etching cleaning and resin/ceramic bonding: microtensile bond strength and EDX analysis

J Adhes Dent. 2010 Aug;12(4):295-303. doi: 10.3290/j.jad.a17709. ABSTRACT PURPOSE: The aim of this study was to evaluate the microtensile bond strength of a resin composite bonded to two heat-pressed ceramics after performing different post-etching cleaning techniques. MATERIALS AND METHODS: Resin composite specimens were bonded to IPS Empress Esthetic (EE) and […]

Micro-raman assessment of the ratio of carbon-carbon double bonds of two adhesive systems cured with LED or halogen light-curing units

J Adhes Dent. 2010 Dec;12(6):461-7. doi: 10.3290/j.jad.a17855. ABSTRACT PURPOSE: the purpose of the study was to compare the ratio of carbon-carbon double bonds (RDB) of two adhesive systems cured by five different light-curing units (LCUs) using micro-Raman spectroscopy. materials and methods: ten samples of an etch-and-rinse (Excite), a two-step self-etching […]

Reducing the incompatibility between two-step adhesives and resin composite luting cements

J Adhes Dent. 2010 Oct;12(5):373-9. doi: 10.3290/j.jad.a17854. ABSTRACT PURPOSE: To determine whether the adverse interaction between a two-step/acidic etch-and-rinse adhesive (One-Step Plus [OS], Bisco) and chemically cured resin luting cement [Variolink II, Ivoclar Vivadent] can improve adhesive coupling by reducing the dentin permeability with an oxalate desensitizer (BisBlock, Bisco). MATERIALS […]

Influence of experimental provisional cements containing zeolite, bone hydroxyapatite and linoleic Acid on bond strength of composite to dentin in vitro

J Adhes Dent. 2010 Dec;12(6):469-75. doi: 10.3290/j.jad.a17727. ABSTRACT PURPOSE: to evaluate the dentin bond strength of a composite resin material after the removal of two experimental cements containing zeolite, bone hydroxyapatite and linoleic acid, and one conventional glass-ionomer cement intended as provisional cements. MATERIALS AND METHODS: forty extracted caries-free, erupted […]

In vitro study of the influence of dentin desensitizing and sealing on the shear bond strength of two universal resin cements

J Adhes Dent. 2010 Oct;12(5):381-92. doi: 10.3290/j.jad.a17714. ABSTRACT PURPOSE: To test whether or not dentin desensitizing or sealing methods influence the bond strength of universal resin cements. MATERIALS AND METHODS: The bond strength of two universal resin cements (RelyXUnicem, Self-adhesive Prototype Cement) to human dentin was assessed after different dentin […]

Marginal quality and fracture strength of root-canal treated mandibular molars with overlay restorations after thermocycling and mechanical loading

J Adhes Dent. 2010 Aug;12(4):287-94. doi: 10.3290/j.jad.a17711. ABSTRACT PURPOSE: To evaluate marginal quality, fracture modes, and loads-to-failure of different overlay restorations in rootcanal treated molars in a laboratory setup. MATERIALS AND METHODS: Thirty-two mandibular first molars were randomly assigned to four groups (n = 8): UTR= untreated (control), RCT-COM= root […]

Mechanical testing of indirect composite materials directly applied on implant abutments

J Adhes Dent. 2010 Aug;12(4):311-7. doi: 10.3290/j.jad.a17710. ABSTRACT PURPOSE: To test the strength to failure and fracture mode of three indirect composite materials directly applied onto Ti-6Al-4V implant abutments vs cemented standard porcelain-fused-to-metal (PFM) crowns. MATERIALS AND METHODS: Sixty-four locking taper abutments were randomly allocated to four groups and were […]